MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Silikony Polskie Polsil Gum 100/60 HTV Silicone Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: Polsil Gum is a general purpose master batch compound, vulcanizing at high temperature after addition of vulcanizing agent. Silicone rubber obtained from Polsil® GUM shows useful properties: ageing resistance, stability of mechanical properties in the range of temperature between -500C and + 2500C, chemical resistance, good insulating properties.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Storage Temperature 0.000 - 40.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60
Tensile Strength at Break >= 8.00 MPa
Elongation at Break 370 - 620 %
Tear Strength >= 17.0 kN/m

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Silastic® 9280/70E KIT PARTS A&B
Applied Silicone 40115 High Consistency Rubber, 50 Durometer (HCRA 4750), Implant Grade
Applied Silicone 40025 Liquid Silicone Rubber, 30 Durometer (LSR 30), Implant Grade
Rogers Arlon CP-375CR Silicone Rubber
Rogers Arlon 10502R020 0.020" (0.508 mm) Cured Silicone Rubber (Unsupported)

PPOLSI015 / 84315

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.