Moplen HP2774 is a polypropylene homopolymer used for extrusion applications. Moplen HP2774 has a very high melt flow rate, a very narrow molecular weight distribution and is in pelletized form. Moplen HP2774 is produced using a non-phthalate Ziegler/Natta catalyst and is used for the production of melt blown nonwovens with outstanding barrier/filtration properties. Moplen HP2774 is also used for compounding applications. Applications: Absorption & Filtration, Hygiene Nonwoven, Nonwovens, Wipes/Tissues.Information provided by LyondellBasell. |