MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Kalrez® 8002 FFKM Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Kalrez® 8002 is a specialty compound targeted specifically for select semiconductor plasma and gas deposition applications. This clear, unfilled compound offers very low particle generation in oxygen and fluorine-based plasmas versus mineral-filled compounds. Kalrez® 8002 exhibits excellent resistance to dry process chemistry, has good mechanical strength properties and is well suited for both static and low stress/low sealing force applications. A maximum continuous service temperature of 250°C (482°F) is suggested. Ultrapure postcleaning and packaging is standard for parts made from Kalrez® 8002.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 69ASTM D 2240
Elongation at Break 256 %ASTM D 412
100% Modulus 2.30 MPaASTM D 412
 
Thermal PropertiesOriginal ValueComments
CTE, linear 395 µm/m-°CISO 11359-1/-2
Maximum Service Temperature, Air 275 °CDuPont proprietary test
Minimum Service Temperature, Air 1.00 °CRetraction temperature TR-10; ASTM D 1329
 
Descriptive Properties
ColorClear
Polymer(FFKM)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Kalrez® 6221 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 8575 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 6375 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 4079 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 6375UP FFKM Perfluoroelastomer

PDVD057 / 33876

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.