MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Unifrax Foamfrax® HD Grade I Fiber HD Insulation
Categories: Ceramic

Material Notes: Foamfrax® HD Insulation is a monolithic thermal management product developed by Unifrax Corporation. This product is a four-component system of specially conditioned bulk ceramic fibers, an inorganic binder, an organic foaming binder, and a clay additive. Foamfrax HD is easily installed. The interlocking network of fibers provides a strong, uniform monolithic structure having excellent thermal insulating properties, very low heat storage, and excellent resistance to thermal shock. Foamfrax HD Insulation is unaffected by most chemicals except hydrofluoric acid, phosphoric acid, and concentrated alkalies.

    Characteristics
  • Speed and ease of installation
  • Low rebound
  • Low thermal conductivity
  • Low thermal shrinkage
  • Low heat storage
  • Excellent thermal shock resistance
  • Good chemical resistance
  • Good sound absorption

    Principal Applications
  • Furnace linings (reformers, boilers, kilns, heat treating furnaces, etc.)
  • Vessel linings
  • Incinerators, flues, ducts and stacks
  • Low mass kiln car decks
  • High-velocity applications
  • Composite lining systems
  • Refractory shapes

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.256 g/cc0.00926 lb/in³Installed Fired
 0.513 g/cc0.0185 lb/in³Installed Wet
Loss On Ignition 0.75 %0.75 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 1760 °C3200 °F
Maximum Service Temperature, Air 1175 °C2147 °FRecommended Operating Temperature
Shrinkage <= 3.0 %
@Time 86400 sec
<= 3.0 %
@Time 24.0 hour
at operating temperature
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 50 %50 %At Installation
 
Descriptive Properties
ColorWhite (Fired)
Temperature Grade (°C)1260

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CUNIF103 / 97875

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.