MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sipol Technipol® 32 Thermoplastic Adhesive Co-polyester
Categories: Polymer; Adhesive; Thermoplastic; Polyester, TP

Material Notes: Description: Technipol® 32 is a co-polyester based thermoplastic adhesive designed for the production of air and oil filters in the automotive industry. Technipol® 32 is characterized by:
  • a high chemical resistance (mineral oil and diesel vapors)
  • a good thermal resistance, compatible with the paper curing temperatures
  • a high flexibility, that assures the integrity of the filter during all production steps

Information provided by SIPOL SpA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ASTM D 792
Viscosity  18 cP
@Temperature 230 °C
18 cP
@Temperature 446 °F
 25 cP
@Temperature 220 °C
25 cP
@Temperature 428 °F
 34 cP
@Temperature 210 °C
34 cP
@Temperature 410 °F
Brookfield Viscosity 34 cP
@Temperature 210 °C
34 cP
@Temperature 410 °F
Cone/ plate Viscometer, Model Brookfield CAP 2000+.; MI 12
Melt Flow 43 g/10 min
@Load 0.325 kg,
Temperature 210 °C
43 g/10 min
@Load 0.716 lb,
Temperature 410 °F
ASTM D 1238
Storage Temperature 5.00 - 10.0 °C41.0 - 50.0 °F
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break >= 500 %>= 500 %ASTM D 638
 
Thermal PropertiesMetricEnglishComments
Melting Point 185 °C365 °FASTM D 3418
 
Processing PropertiesMetricEnglishComments
Processing Temperature 100 - 120 °C212 - 248 °FUnder Hopper
 180 - 210 °C356 - 410 °FCompression Zone
 220 - 240 °C428 - 464 °FMetering Zone
Feed Temperature 140 - 160 °C284 - 320 °F
Nozzle Temperature 240 - 250 °C464 - 482 °F
Die Temperature 240 - 250 °C464 - 482 °F
Shelf Life 12.0 Month12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSIPOL003 / 297128

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.