MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

M. Holland Company MAGMA® LM233-A LLDPE  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: Features: Good Heat Seal, Good Processability

Uses: Coating Applications, Film, Cast Film, Packaging

Processing Method: Coextrusion, Blown Film

Information provided by M. Holland.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.903 g/cc0.0326 lb/in³ASTM D792
Melt Flow 7.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Neck In 12.7 cm5.00 inat 280°C, 1.0 mil
 
Thermal PropertiesMetricEnglishComments
Melting Point 97.2 °C207 °FASTM D3218
 
Optical PropertiesMetricEnglishComments
Haze 1.5 %1.5 %ASTM D1003
Gloss 94 %94 %at 45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 88.9 °C192 °FSeal Initiation Temp
Feed Temperature <= 149 °C<= 300 °F
Melt Temperature 182 - 199 °C360 - 390 °F
 302 °C575 °FSuggested for extrusion coating only
Blow-up Ratio (BUR) 2.0 - 3.02.0 - 3.0
 
Descriptive Properties
Adhesion to PP Films0.98at 280°C
FormPellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1010 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round or thickness
AISI 1010 Steel, CQ sheet,1.6-5.8 mm round or thickness
AISI 1010 Steel, cold drawn bar, 19-32 mm (0.75-1.25 in) round or thickness
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel

PMH086 / 53019

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.