MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ASI® Pipe Sealer Torque 60 RC Anaerobic Urethane Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: Torque 60 RC is a high viscosity gap filling silver paste used between machinery parts to repair worn areas and restore correct fits. It repairs worn shaft and housing, bearing spinouts, wallowed keyways and splines, threaded parts. Highly resistant to heat, vibrations, corrosion, water, gas, oil hydrocarbons many chemicals.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/cc
@Temperature 25.0 °C
uncured
Brookfield Viscosity 150000 - 350000 cP
@Temperature 25.0 °C
Uncured. Spindle TB- 5 rpm
 1.00e+6 - 2.00e+6 cP
@Temperature 25.0 °C
Uncured. Spindle TB-0.5 rpm
Storage Temperature 8.00 - 28.0 °Cuncured
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 16.0 - 26.0 psi24 hrs 20° on steel; DIN 54452
 15.0 - 30.0 psi24 hrs 20° on steel; ISO 10123
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C@ 20° on steel 24 hrs; ASTM D696
Specific Heat Capacity 0.300 J/g-°C20° on steel 24 hours. Cured
Thermal Conductivity 0.100 W/m-K
@Time 86400 sec
Cured. 20° on steel; ASTM C177
Maximum Service Temperature, Air 150 °CBolt M 10x20 quality 8.8-nut h=0.8d
Minimum Service Temperature, Air -55.0 °CBolt M 10x20 quality 8.8-nut h=0.8d
Flash Point >= 93.0 °Cuncured
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 20.0 °C
uncured
 
Descriptive Properties
Chemical ClassUrethane Methacrylate
Color / appearanceGray paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASINC9205 / 233571

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.