MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ganpati Exim Group III PBR ND
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: PBR Nd is a product of butadiene solution polymerization with neodymium compounds used as a catalyst. This rubber is used for production of tires, rubber-technical articles and in other areas of application. PBR Nd is gel free, cis chains content is at least 96%.

Application: The Poly-butadiene SKD rubber is applied in tire, rubber-technical and asbestos-technical industries. It is easy compatible with natural and butadiene-styrene rubbers in any properties. This property is very important for the production of SKD based products.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 60 - 70
@Temperature 100 °C
60 - 70
@Temperature 212 °F
ML (1+4)
Ash <= 0.50 %<= 0.50 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 20.0 MPa>= 2900 psi
Elongation at Break >= 450 %>= 450 %
300% Modulus >= 9.00 MPa>= 1310 psi
Rebound >= 0.51 %>= 0.51 %elasticity
 
Descriptive Properties
Coldflow<10 mm/h
Content0.6-1.0%Agidol-2 mass content
Mass losses at drying<0.5%
Plasticity0.4-0.5
Viscosity Scattering<5%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGANPATI031 / 317315

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.