MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman ComAlloy Lubrilon® 620 Nylon 6/6, Glass Fiber/Molybdenum Disulfide Filled, Flow Enhanced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber/MoS2 Filled

Material Notes: Data provided by the manufacturer, ComAlloy International Company.

High performance and excellent lubricity with minimal surface wear.

The ComAlloy product line has been integrated into the A Schulman product line.

Key Words: Polyamide 6/6; Polyamide 66; Nylon 66; ComAlloy International Company, subsidiary of A. Shulman Inc.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.53 g/cc
Linear Mold Shrinkage 0.0020 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ASTM D785
Tensile Strength, Ultimate 165 MPaASTM D638
Elongation at Break 2.0 %ASTM D638
Flexural Strength 253 MPaASTM D790
Flexural Modulus 12.9 GPaASTM D790
Izod Impact, Notched 0.690 J/cmASTM D256
Izod Impact, Unnotched 7.47 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 255 - 275 °C
Deflection Temperature at 0.46 MPa (66 psi) 253 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 248 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 271 - 285 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röchling Fibracon® PTFE + 55% Bronze + 5% MoS2
Röchling Fibracon® PTFE + 15% Glass + 5% MoS2
Daikin POLYFLON MG-1431F PTFE 20% Glass Fiber and 5% MoS2 Filled Molding Powder, High Apparent Density, Free Flow
AGC Fluon® RB1211 15% Glass Fiber, 5% MoS2, PTFE Filled Compound
AGC Fluon® PB1211 15% Glass Fiber, 5% MoS2, PTFE Filled Compound

PASH1F / 24814

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.