Europrene® 1605 is a carbon black masterbatch obtained by adding N 550 carbon black to an emulsion styrene-butadiene latex before coagulation. The latex is obtained by cold polymerization using a mixture of rosin acid and fatty acid soaps as emulsifiers. A non-staining antioxidant is added during the production process. Key Features: The use of black masterbatch offers many benefits to the manufacturer such as: shorter mixing cycles with higher capacity; reduced energy demand; improved carbon black dispersion; cleaner plant environment. Main Applications: Calendered and extruded technical articles, soles. Information provided by Polimeri Europa. Versalis is the Eni subsidiary containing the plastics and rubber businesses. |