MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Versalis Europrene® 1605 Emulsion Styrene-Butadiene Rubber - Cold Black Masterbatch  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Europrene® 1605 is a carbon black masterbatch obtained by adding N 550 carbon black to an emulsion styrene-butadiene latex before coagulation. The latex is obtained by cold polymerization using a mixture of rosin acid and fatty acid soaps as emulsifiers. A non-staining antioxidant is added during the production process.

Key Features: The use of black masterbatch offers many benefits to the manufacturer such as: shorter mixing cycles with higher capacity; reduced energy demand; improved carbon black dispersion; cleaner plant environment.

Main Applications: Calendered and extruded technical articles, soles.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.60 %<= 0.60 %ASTM D5668
Ash <= 0.40 %<= 0.40 %ASTM D5667
 
Chemical PropertiesMetricEnglishComments
Styrene Content 23.5 %23.5 %Bound; ASTM D5775
 
Descriptive Properties
Carbon Black Loading (phr)50
Organic Acid3.5% wtASTM D5774
Soap< 0.5% wt

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Versalis Europrene® 1609 T Emulsion Styrene-Butadiene Rubber - Cold Black Masterbatch
Versalis Europrene® 1606 T Emulsion Styrene-Butadiene Rubber - Cold Black Masterbatch

PENG172 / 124566

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.