MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ALM TPE 360 CoPolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: This CoPolyester material has excellent physical properties, is easy to process and has 100% recyclability.

Highlights:

  • 100% recyclable
  • Soft, white parts out of the machine
  • Easy to process
  • Toughness and flexibility
Applications:
  • Footwear
  • Automotive gaskets and seals
  • Cushioning applications
  • Ideal for applications requiring softer parts with excellent ductility and surface finish

Information provided by Advanced Laser Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.990 g/cc0.0358 lb/in³
Particle Size 44.6 µm44.6 µmDv 10
 80.4 µm80.4 µmDv 50
 130 µm130 µmDv 90
Viscosity 897000 cP
@Temperature 220 °C
897000 cP
@Temperature 428 °F
1 rad/s
Molecular Weight 5968 g/mol5968 g/molMn
 31129 g/mol31129 g/molMw
 69961 g/mol69961 g/molMz
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9494ASTM D2240
Tensile Strength, Ultimate 14.0 MPa2030 psiZ; ASTM D638
 17.0 MPa2470 psiXY; ASTM D638
Elongation at Break 28 %28 %Z; ASTM D638
 129 %129 %XY; ASTM D638
Tensile Modulus 0.134 GPa19.4 ksiZ; ASTM D638
 0.143 GPa20.7 ksiXY; ASTM D638
Tear Strength 103 kN/m588 pliASTM D624
Taber Abrasion, mg/1000 Cycles 67
@Load 1.00 kg
67
@Load 2.20 lb
[mg{, CS-17; ASTM D4060
Compression Set 59.5 %
@Temperature 70.0 °C,
Time 79200 sec
59.5 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Melting Point 304.37 °C579.87 °F
Crystallization Temperature 149.72 °C301.50 °F
 
Descriptive Properties
Enthalpy19.62 J/gmelting
 21.46 cal/gcrystallization

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PALP9012 / 312347

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.