MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chambroad Petrochemicals IIR1953 Ordinary Butyl Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Ordinary Butyl Rubber: Ordinary butyl rubber (isobutene-isoprene rubber, IIR) has a small unsaturated portion of the molecular chain, wide distribution of methyl in the side chain, good air tightness, low energy absorption capacity, chemical stability, and thermal stability. It is used in inner tubes of tires, vulcanized bladders, waterproof materials, and shock absorption materials.

Information provided by Shandong Chambroad Petrochemicals Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.30 %<= 0.30 %mass fraction, High-quality product
 <= 0.50 %<= 0.50 %mass fraction, Acceptable
Mooney Viscosity  46 - 51
@Temperature 125 °C
46 - 51
@Temperature 257 °F
(1+8), Acceptable
 48 - 54
@Temperature 125 °C
48 - 54
@Temperature 257 °F
(1+8), High-quality product
Ash <= 0.30 %<= 0.30 %mass fraction
 
Descriptive Properties
AppearanceWhite solid block
Content>0.03Antioxidant
Vulcanization characteristics1-3 minTs1
 15.4-18.2 dN-mFH
 17.1-23.7 minT90
 2.4-4.2 dN-mFL
 3.3-7.3 minT50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHAMB060 / 318602

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.