MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Geniosil® GF 31 Silane
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Empirical formula: C10H20O5Si

CAS No.: 2530-85-0

Properties: The use of GENIOSIL® GF 31 as a coupling agent in glass fiber-reinforced or filler-modified plastics improves filler dispersibility while reducing the filler's sedimentation tendency. It also results in a major reduction in the melt viscosity of casting resins, as well as a marked improvement in the mechanical properties of glass-fiber-reinforced or mineral-filled plastics.In addition, use of GENIOSIL® GF 31 in these materials leads to a sizable increase in moisture (vapor) resistance as well as greater resistance to acids and bases. Used as a co-monomer in polymers, GENIOSIL® GF 31 produces binders that exhibit much improved wet scrub, abrasion and scratch resistance thanks to crosslinking and strong adhesion to the base.As a component of free-radical curable adhesives and sealants, GENIOSIL® GF 31 leads to improved mechanical properties and enhanced substrate adhesion.

Special features: GENIOSIL® GF 31 is an alkoxysilane with a methacrylic organofunctional group.It is a clear, colorless, light and heat sensitive liquid with a characteristically sweet odor. The silane hydrolyzes in the presence of moisture (methanol is released) to form silanols, which can then react with themselves to produce siloxanes. As a bifunctional, organically unsaturated molecule, GENIOSIL® GF 31 can be incorporated into organic polymers, e.g. via radical grafting.

Application: GENIOSIL® GF 31 is mainly used in glass fiber or glass fabric-reinforced polyester and polyolefin molded components. GENIOSIL® GF 31 is used as a surface modifier for fillers and pigments used in thermosetting plastics, thermoplastics, and elastomers, as well as a polymer component in surface coatings. Further important areas of application are heat and/or radiation-curable adhesives and sealants..

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³DIN 51757
Viscosity 2.6 cP2.6 cPdynamic
Molecular Weight 248.4 g/mol248.4 g/mol
 
Thermal PropertiesMetricEnglishComments
Boiling Point >= 125 °C
@Pressure 0.00150 MPa
>= 257 °F
@Pressure 0.218 psi
Flash Point >= 100 °C>= 212 °FISO 2719
Ignition Temperature 265 °C509 °Fliquids; DIN 51794
 
Descriptive Properties
Content<30 mg/kgHydrolyzable chloride (as HCl)
Purity>98%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9310 / 204839

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.