MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Teijin Tenax® E TPUD PEEK-IMS65 Composite
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Tenax®-E TPUD PEEK-IMS65 is a Thermoplastic Unidirectional prepreg (TPUD) which combines two high-performance materials. The polymer matrix of PEEK (polyetheretherketone) offers excellent resistance to chemicals and solvents and the utilization of Tenax®-E IMS65 a high tenacity intermediate modulus carbon fiber manufactured with a tailored sizing for thermoplastics applications, result in a composite offering outstanding material performance.

Product Benefits

  • High-performance mechanical properties
  • Tailored thermoplastic sizing
  • Continuous use at elevated temperature
  • Low flammability, smoke and toxicity
  • Resistant to chemicals and solvents
  • Room temperature storage and shipping
  • Compliant to Health, Safety and Environment requirements
Process Benefits
  • Out of autoclave consolidation (press forming, tape winding)
  • Short cycle time
  • Thermo-formable
  • Automated process (AFP, ATL)
  • Thermoplastic joining technologies

Information provided by Teijin Carbon America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.78 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 78.4 ksiOpen Hole (QI); ASTM D5766
 386.5 ksi(0°); ASTM D3039
Tensile Modulus 2280 ksi(0°); ASTM D3039
Flexural Strength 7.38 ksi(90°); ASTM D790
Compressive Strength 43.3 ksiOpen Hole (QI); ASTM D6484
 105.8 ksi(90°/0°); ASTM D6641
Compressive Modulus 1100 ksi(90°/0°); ASTM D6641
 2130 ksi(0°); ASTM D6641
Shear Modulus 690 ksiIn Plain Shear; ASTM D3518
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 147 °Conset; ASTM D3418

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEIJIN924 / 277934

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.