MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wellman Wellamid® MR409 22H-N 40% Mineral Reinforced Nylon 66, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Mineral Filled

Material Notes: Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive cooling fans & shrouds, automotive door handles, brackets, automotive mirror shells, painted parts, components for small gas engines, sporting goods, auto luggage rack components.

Data provided by the manufacturer, Wellman Inc.

Key Words: Polyamide 66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³ISO 1183
Water Absorption 0.70 %0.70 %Approximate 24 hr.
Linear Mold Shrinkage 0.010 - 0.014 cm/cm0.010 - 0.014 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 85.0 MPa12300 psiISO 527
Elongation at Break 6.0 %6.0 %ISO 527
Flexural Yield Strength 140 MPa20300 psiISO 178
Flexural Modulus 5.70 GPa827 ksiISO 178
Izod Impact, Notched 0.600 J/cm1.12 ft-lb/inISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FISO 75
Flammability, UL94 HB
@Thickness 0.790 mm
HB
@Thickness 0.0311 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 282 - 304 °C540 - 580 °F
Middle Barrel Temperature 277 - 299 °C530 - 570 °F
Front Barrel Temperature 271 - 293 °C520 - 560 °F
Nozzle Temperature 282 - 293 °C540 - 560 °F
Melt Temperature 288 - 310 °C550 - 590 °F
Mold Temperature 71.1 - 93.3 °C160 - 200 °F
Drying Temperature 79.4 °C175 °FOpened bags and gaylord boxes
Dry Time 2 - 4 hour2 - 4 hourOpened bags and gaylord boxes
Moisture Content 0.050 - 0.20 %0.050 - 0.20 %During molding to prevent hydrolytic degradation
 <= 0.20 %<= 0.20 %In shipping bags, ready to mold
Injection Pressure 34.5 - 138 MPa5000 - 20000 psi
Back Pressure 0.345 MPa50.0 psi
Screw Speed 30 - 120 rpm30 - 120 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWEL38 / 72318

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.