MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Westlake EPOLENE® E-20P Low Molecular Weight Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: EPOLENE® E-20P is an oxidized low molecular weight polyethylene powder with exceptional hardness and low color used in emulsify able applications. The low softening point and low viscosity contribute to the hardness, short drying time, and excellent gloss in coatings. Pressure equipment is required for emulsification of this material. EPOLENE® E20P polymer is an excellent performer in high-speed buff able floor finishes. It improves buff ability and durability. Applications: Compounding, PVC lubrication, Emulsions, Wax Modification. Attributes: Imparts slip resistances, durability, and toughness to floor finishes, Oxidized to provide functionality for PVC lube, Produces stable water based emulsions, Useful as a lubricant for HDPE extrusion, Oxidized low density polyethylene powder.

All tests are run at 23°C (73°F) and 50% relative humidity.

Information provided by Westlake Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 215 µmMedian; Westlake
Brookfield Viscosity 1000 - 2000 cP
@Temperature 125 °C
ASTM D4287
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 14 - 18.5mg-KOH/g; ASTM D1386
 
Thermal PropertiesOriginal ValueComments
Dropping Point 108 - 116 °CMettler; ASTM D6090
 
Optical PropertiesOriginal ValueComments
Yellow Index <= 4.0 %ASTM E313
 
Descriptive Properties
Penetration Hardness<1 dmmASTM D5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWESF8716 / 287826

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.