MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Petropol Thanelene® A3 90A HL PRTA010 TP302 MSP TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Product Description: Hardness 90 shore A, Plasticized, Thermoplastic Polyurethane

Resin ID (ISO 1043): TPU
Additive: Plasticized
Processing: Injection Molding, Extrusion
Color: Black

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9393ISO 7619-1
Hardness, Shore D 4141ISO 7619-1
Tensile Strength at Break >= 50.0 MPa>= 7250 psiDIN 53504
Tensile Stress  10.0 MPa
@Strain 100 %
1450 psi
@Strain 100 %
DIN 53504
 19.0 MPa
@Strain 300 %
2760 psi
@Strain 300 %
DIN 53504
Elongation at Break 550 %550 %DIN 53504
Tensile Modulus  0.0450 GPa
@Temperature 60.0 °C
6.53 ksi
@Temperature 140 °F
Storage; ISO 6721-1
 0.0900 GPa
@Temperature 20.0 °C
13.1 ksi
@Temperature 68.0 °F
Storage; ISO 6721-1
 0.450 GPa
@Temperature -20.0 °C
65.3 ksi
@Temperature -4.00 °F
Storage; ISO 6721-1
Resilience 3030[%], Impact Resilience; ISO 4662
Abrasion <= 30<= 30[mm3]; ISO 4649
Compression Set  25 %
@Temperature 23.0 °C,
Time 259000 sec
25 %
@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
 40 %
@Temperature 70.0 °C,
Time 86400 sec
40 %
@Temperature 158 °F,
Time 24.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 225 °C410 - 437 °F
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F
Drying Temperature 90.0 °C194 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPETROPOL401 / 313309

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.