Product description: Grilon CF 6 S is an extracted copolyamide with a low melting point.- Very high flexibility and toughness
- Very good thermoforming and orientation properties
- High shrink
- Very good transparency
- Low melting point (130°C)
Grilon CF 6 S is suitable for the manufacture of both flat and blown coextruded films with temperature sensitive polymers such as PVDC and EVOH. Typical applications are cook in bag for meat, cheese, deep-draw consumer and medical packaging and asymmetric barrier film structures.Information provided by EMS Grivory. |