MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ATI Allegheny Ludlum AL 20™ Plate Specialty Steel
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: The N08020 alloy has been available for many years and has found applications in many environments, such as in chlorides and in sulfuric and sulfurous acids.

Although AL 20 alloy was developed for improved resistance to corrosion by sulfuric acid, it fins wide use throughout the chemical industry. It is used extensively in the manufacture of solvents, explosives, plastics, synthetic fibers, organic chemicals, pharmaceuticals, and food-processing equipment. Containment of acid mixtures and chloride stress corrosion resistance are examples of successful applications for AL 20 alloy. Where purity must be maintained in the processing of products such as foodstuffs or dyes, AL 20 alloy is used to protect end products from the danger of contamination by metallic ions through corrosion.

AL 20 alloy has been applied economically in many areas where other materials my provide the necessary corrosion resistance, but are either higher in initial cost or more expensive to install and maintain. Important advantages of AL 20 alloy are its excellent mechanical properties and comparative ease of fabrication. The presence of columbium in the alloy minimizes the precipitation of carbides in heat-affected zones during welding so that assemblies can usually be placed in service in the as-welded condition. Welds with matching filler metal will be slightly less corrosion resistant than the base alloy.

The N08020 alloy is readily available in a wide range of product forms, and is covered by a wide variety of ASTM and ASME specifications having assigned maximum working stresses to 540 °C. The alloy is familiar to many fabricators and the weldability of this alloy contributes to its use in many engineered applications. Weld filler metal is readily available and welding procedures are well established.

Information provided by Allegheny Ludlum

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.08 g/cc0.292 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 200 - 220200 - 220typical plate
Tensile Strength, Ultimate 85.0 - 95.0 MPa12300 - 13800 psiTypical
Tensile Strength, Yield 50.0 - 60.0 MPa7250 - 8700 psiTypical
Elongation at Break 35 - 45 %35 - 45 %Typical
Modulus of Elasticity 193 GPa28000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000108 ohm-cm0.000108 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  14.7 µm/m-°C
@Temperature 20.0 - 100 °C
8.17 µin/in-°F
@Temperature 68.0 - 212 °F
 15.4 µm/m-°C
@Temperature 20.0 - 250 °C
8.56 µin/in-°F
@Temperature 68.0 - 482 °F
Specific Heat Capacity 0.500 J/g-°C0.120 BTU/lb-°F
Thermal Conductivity 12.2 W/m-K84.7 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.020 %0.020 %
Chromium, Cr 19.5 %19.5 %
Copper, Cu 3.2 %3.2 %
Iron, Fe 41 %41 %as balance
Manganese, Mn 0.40 %0.40 %
Molybdenum, Mo 2.15 %2.15 %
Nickel, Ni 33 %33 %
Niobium, Nb (Columbium, Cb) 0.40 %0.40 %includes Ta
Phosphorus, P 0.025 %0.025 %
Silicon, Si 0.40 %0.40 %
Sulfur, S 0.0020 %0.0020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NLN20B / 18011

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.