MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chesterton ARC S7 AR Ceramic-Filled Industrial Coating
Categories: Polymer; Thermoset; Vinyl Ester

Material Notes: ARC S7 AR is a novolac vinyl ester based, ceramic reinforced, protective coating for high temperature, chemical exposures where erosive particulates and thermal cycling conditions may be present.

ARC S7 AR is designed to: Resist erosion; Resist thermal cycling conditions up to 180°C (350°F); Resist a wide range of inorganic as well as organic acids and hydrocarbon based chemical compounds; Easily apply by airless spray system

Matrix: An epoxy novolac vinyl ester resin reacted with a catalyst. Filler: A proprietary blend of high density ceramic and glass flake reinforcements.

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³Cured
Volatile Organic Compounds (VOC) Content 10 g/l
@Treatment Temp. 110 °C
10 g/l
@Treatment Temp. 230 °F
Part A and B; EPA 24
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585ASTM D2240
Elongation at Break 2.37 %2.37 %ASTM D638
Flexural Strength 50.3 MPa7300 psiASTM D790
Flexural Modulus 3.24 GPa470 ksiASTM C580
Compressive Strength 488 MPa70800 psiASTM D695
Adhesive Bond Strength 25.5 MPa3700 psiPull-Off Adhesion; ASTM D4541
Impact Test >= 2.26 J>= 1.67 ft-lbDirect; ASTM D2794
Taber Abrasion, mg/1000 Cycles 278
@Load 1.00 kg
278
@Load 2.20 lb
H-18 Wheel; ASTM D4060
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 135 °C275 °FWater
 180 °C356 °FContinuous Dry Service
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature 10.0 - 32.0 °C
6.00 Month
@Temperature 50.0 - 89.6 °F
Dry, Unopened Containers
 
Descriptive Properties
ColorLight Gray or Dark Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type S7 Tool Steel (UNS T41907)
Bohler-Uddeholm COMPAX™ AISI S7 MOLD QUALITY Cold Work Steel
ATI Allegheny Ludlum S7 Tool Steel, UNS T41907
EDRO #7 Shock Resistant S7 Tool Steel
Crucible Steel S7 XL (Premium AISI S7) Tool Steel

PPTCHS037k / 239859

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.