MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Skamol Group Moler POROS Insulating Block
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: SKAMOL Moler insulating bricks & blocks have the following characteristics:
  • Max. service temperature: Up to 1000°C (1832°F)
  • Back-up insulation
  • Excellent insulating properties
  • High mechanical strength
  • Light weight
  • Good thermal shock resistance
  • Increasing strength at rising temperatures
  • High content of amorphous silica accounting for an increased viscosity being induced into attacking slags or melts
  • Non-wetting to molten aluminum and other metals
  • A wide range of bricks and blocks in various combinations of bulk density, thermal conductivity and crushing strength
  • Primarily used for back-up insulation, typically in industrial furnaces behind a refractory lining.

Information provided by Skamol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.625 g/cc0.0226 lb/in³Dry
Loss On Ignition 1.0 %
@Temperature 1025 °C
1.0 %
@Temperature 1877 °F
Porosity 74 %74 %Total
Permeability 9.09.0nPm, Permeability to Air; BS EN 993-4: 1995
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.000700 GPa0.102 ksiEN 993-6: 1995
Compressive Strength 2.50 MPa363 psiEN 1094-5: 1995
 
Thermal PropertiesMetricEnglishComments
CTE, linear 2.00 µm/m-°C
@Temperature 20.0 - 750 °C
1.11 µin/in-°F
@Temperature 68.0 - 1380 °F
BS 1902: section 5.3: 1990
Specific Heat Capacity 0.800 J/g-°C0.191 BTU/lb-°F
Thermal Conductivity  0.132 W/m-K
@Temperature 200 °C
0.916 BTU-in/hr-ft²-°F
@Temperature 392 °F
Mean temp.; ASTM C-182
 0.149 W/m-K
@Temperature 400 °C
1.03 BTU-in/hr-ft²-°F
@Temperature 752 °F
ASTM C-182
 0.169 W/m-K
@Temperature 600 °C
1.17 BTU-in/hr-ft²-°F
@Temperature 1110 °F
ASTM C-182
Maximum Service Temperature, Air 900 °C1650 °F
Shrinkage 1.0 %
@Temperature 1000 °C,
Time 43200 sec
1.0 %
@Temperature 1830 °F,
Time 12.0 hour
Linear Reheat Shrinkage; EN 1094-6: 1999
 
Component Elements PropertiesMetricEnglishComments
Al2O3 9.0 %9.0 %
CaO 0.80 %0.80 %
Fe2O3 7.0 %7.0 %
K2O 1.6 %1.6 %
MgO 1.3 %1.3 %
Na2O 0.40 %0.40 %
SiO2 77 %77 %
SO3 1.2 %1.2 %
TiO2 0.70 %0.70 %
 
Descriptive Properties
ColorRed
Creep in Compression0.7%BS EN 993-9: 1997, after fluoride gas exposure, 50h at 800°C (1472°F), load 0.1 MPa (14.5 psi)
Pyrometric Cone Equivalent1350°CASTM C24-89, ORTON cones
Resistance to Thermal ShockMin 30 cyclesEN 993-11: 1998, heating to 950°C (1742°F)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CSKAM006 / 2157

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.