MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Powersil® INSULATOR FINISH Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: POWERSIL® INSULATOR FINISH is a self leveling, one-component silicone rubber, which cures at room temperature under the influence of moisture in the air. The elastomer has good mechanical and very good electrical properties.

Special features:

  • acetic acid-curing system
  • self-leveling
  • tracking and erosion resistant
  • excellent primerless adhesion to many substrates
  • very good resistance to weathering and air pollution
Application: Repair material for silicone rubber sheds and housings of long rod and hollow core insulators, arresters and bushings.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³in water; ISO 2781
Viscosity 800000 cP800000 cPdynamic
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2020ISO 868
Tensile Strength at Break 1.40 MPa203 psiISO 37
Elongation at Break 500 %500 %ISO 37
Tear Strength 5.00 kN/m28.5 pliASTM D624 B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Dielectric Constant 3.0
@Frequency 50 Hz
3.0
@Frequency 50 Hz
IEC 60250
Dielectric Strength 20.0 kV/mm508 kV/inIEC 60243
 
Processing PropertiesMetricEnglishComments
Cure Time 600 - 1800 min
@Treatment Temp. 23.0 °C
10.0 - 30.0 hour
@Treatment Temp. 73.4 °F
per mm, 50% RH
 
Descriptive Properties
Colorlight graycured
 light grayuncured
Track Resistance1A 3.5IEC 60587

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9394 / 204923

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.