MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Amity Thermosets ATO 142 Phenolic Molding Organic Filler, Compression Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic

Material Notes:

Characteristics:

  • Electrical low loss
  • Good mechanical strength
  • High electrical insulation
  • Good mechanical strength
  • Glossy surface
  • Low water absorption
  • Color-black, brown
  • Medium/hard flow
  • Applications:

  • Electric switchgear components ( eg. relays )
  • Telecommunication equipment parts
  • Electronic equipment parts
  • Automotive ( electronic and electrical ) parts
  • Medium tension pulleys
  • High gloss toilet seats
  • Big meter covers
  • Circuit breaking switches
  • Coffee machine bases
  • Automobile light and signaling switches
  • Moulding which ought to have overall good properties
  • Solenoid switch covers, knobs and tops (superior quality), etc.
  • Information provided by Amity Thermosets Limited

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 1.35 - 1.38 g/ccMolding; IS 867-1963
    Apparent Bulk Density 0.620 - 0.680 g/ccIS 867-1963
    Water Absorption 0.30 - 0.40 %IS 13411-1993
    Linear Mold Shrinkage 0.0075 - 0.0083 cm/cmIS 13411-1992
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength at Break 50.0 - 60.0 MPa5 mm/min.; IS 867-1963
    Shear Strength 70.0 - 84.0 MPaIS 867-1963
    Izod Impact, Notched 25.0 - 40.0 J/mIS 13411-1992
     
    Electrical PropertiesOriginal ValueComments
    Volume Resistivity 3.16e+10 - 3.16e+11 ohm-cmIS 3396-1979
    Surface Resistance 1.00e+10 - 1.00e+11 ohmIS 3396-1979
    Dielectric Strength 5.50 - 7.50 kV/mm
    @Temperature 90.0 °C
    IS 2584-1963
    Comparative Tracking Index >= 125 V2824-1975
     
    Processing PropertiesOriginal ValueComments
    Mold Temperature 160 - 180 °C
    Injection Pressure 15.68 - 34.3 MPaMold Pressure
    Cure Time 20.0 - 25.0 secper mm
    Shelf Life 12.0 Month10-25°C

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Amity Thermosets ATO 1510 Phenolic Molding Glass fiber Filler, Compression Molded
    Amity Thermosets ATO 145 Phenolic Molding Organic Filler, Compression Molded
    Amity Thermosets ATM 144 Phenolic Molding Organic Filler, Compression Molded
    Amity Thermosets ATM 125 Phenolic Molding Organic Filler, Compression Molded
    Amity Thermosets ATM 123 Phenolic Molding Organic Filler, Compression Molded

    PAMITY14 / 24042

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.