MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Santoprene® 8201-90 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A hard, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of applications. This grade of Santoprene 8000 TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.

Key Features:

  • Non-hygroscopic product, requires little to no drying before processing.
  • Neutral, easy coloring formulation.
  • Recommended for applications requiring excellent ozone resistance.
  • Used in sealing applications.
  • Recommended for applications requiring excellent flex fatigue resistance.
  • UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified For Canada - Component.
  • Although not NSF certified, this product has a Material Supplier Form on file with NSF to facilitate its evaluation for use in applications requiring NSF certification.
  • EU and China RoHS compliant.
Applications:
  • General Purpose
Uses:
  • Appliance Components
  • Cell Phones
  • Flexible Grips
  • Kitchenware
  • Stationary Supplies
  • Strain Reliefs
Processing Method: Blow Molding, Coextrusion, Extrusion, Extrusion Blow Molding, Injection Blow Molding, Injection Molding, Multi Injection Molding, Profile Extrusion, Sheet Extrusion, Thermoforming and Vacuum Forming

Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Key Words: EU 2003/11/EC; RoHS Compliant; UL QMFZ2; UL QMFZ8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 962 mm, 15 sec; ISO 868
 97Air at 302°F, 168 hr; ASTM D573
Tensile Strength at Break 1890 psiAcross Flow; ASTM D412
 1910 psiAir at 302°F, 168 hr; ASTM D573
Tensile Stress at Strain 1030 psi
@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 527 %Air at 302°F, 168 hr; ASTM D573
 620 %Across Flow; ASTM D412
Tear Strength 274 pli73°C, Die C; ASTM D624
Compression Set 52 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -65.0 °FASTM D746
UL RTI, Electrical 100 °CUL 746
UL RTI, Mechanical with Impact 90.0 °C
@Thickness 1.10 mm
UL 746
 95.0 °C
@Thickness 1.60 mm
UL 746
 95.0 °C
@Thickness 3.00 mm
UL 746
Flammability, UL94 HB
@Thickness 1.10 mm
 HB
@Thickness 1.60 mm
 HB
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 175 - 230 °C
Rear Barrel Temperature 375 - 400 °F
Middle Barrel Temperature 385 - 410 °F
Front Barrel Temperature 385 - 410 °F
Nozzle Temperature 410 - 430 °F
Die Temperature 385 - 435 °FExtrusion
Melt Temperature 390 - 420 °FProcessing
 385 - 435 °FExtrusion
Mold Temperature 75.0 - 125 °FProcessing
Moisture Content 0.080 %
Back Pressure 50.0 - 100 psi
Clamp Pressure 6000 - 10000 psi
Vent Depth 0.00100 in
Cushion 0.125 - 0.250 in
Screw Speed 100 - 200 rpm
 
Descriptive Properties
Change in Mass in Air-7.0%150°C, 168 hr, ASTM D573
ColorNatural Color
FormPellets
Injection RateFast
Maximum Regrind %20
Screw Compression Ratio2:1 - 2.5:1
Screw L/D Ratio16:1 - 20:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 8201-80 Thermoplastic Elastomer
ExxonMobil Santoprene® 8201-80HT Thermoplastic Elastomer
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer
ExxonMobil Santoprene® 8201-70 Thermoplastic Elastomer
ExxonMobil Santoprene® 8191-55B100 Thermoplastic Elastomer

PADVA007 / 22697

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.