MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

CHT AS1803 RTV, silicone adhesive sealant
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Description: This is a non-corrosive, neutral cure, 1-part, RTV (Room Temperature Vulcanizing) silicone adhesive sealant. It is one in a range of Acetone cure products which are solvent free. It exhibits excellent primerless adhesion to many substrates and cures rapidly at room temperature when in contact with atmospheric moisture to form a tough rubber. This product will not corrode copper or its alloys and is suitable for use with electronic components.

Key Features

  • UL recognized in file No. E334038
  • Good thermal conductivity
  • Non corrosive
  • Fast skinning
Cured Product: 7 days at 23+/-2°C and 50+/-5% humidity

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.24 g/cc0.0809 lb/in³BS ISO 2781
Linear Mold Shrinkage 0.010 cm/cm0.010 in/in
Storage Temperature <= 40.0 °C<= 104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565ASTM D2240-95
Tensile Strength 2.80 MPa406 psiISO 37
Elongation at Break 94 %94 %ISO 37
Tensile Modulus 0.000400 GPa0.0580 ksiYoung's
100% Modulus 0.503 MPa73.0 psi
Shear Strength 0.255 MPa37.0 psiLap Shear Stainless Steel; ASTM D1002
 0.294 MPa42.6 psiLap Shear Copper; ASTM D1002
 0.588 MPa85.3 psiLap Shear Aluminum; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D-257
Dielectric Constant 4.94.9ASTM D-150
Dielectric Strength 20.0 kV/mm508 kV/inASTM D-149
Dissipation Factor 0.00900.0090ASTM D-150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 198 µm/m-°C110 µin/in-°F
Thermal Conductivity 1.55 W/m-K10.8 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 220 °C428 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 4.00 min0.0667 hourTooling Time
 480 min
@Temperature 23.0 °C
8.00 hour
@Temperature 73.4 °F
3mm Depth
Shelf Life 9.00 Month9.00 Monthin cartridges
 12.0 Month12.0 Monthin pails drums
 
Descriptive Properties
ColorWhite
Cure typeAcetone
RheologyPaste
Self BondingYes
Volume Coefficient of Thermal Expansion475 ppm/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL031 / 314514

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.