MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
PBI Performance Products Celazole® TL-60 Self Lubricating Melt Processable Polybenzimidazole
Categories: Polymer; Thermoplastic; Polybenzimidazole (PBI)

Material Notes: Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. Celazole® T-Series products combine the superior mechanical properties and thermal resistance of PBI with the melt process ability of polyaryletherketones.
Designed for injection molding and extrusion
Celazole TL-60 is a lube grade blend offering superior wear resistance, low friction, chemical resistance and high load bearing capability. Well-suited for rotor vanes, thrust bearings, plane bearings, bushings and other friction management applications – particularly under load.

Information provided by PBI Performance Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.43 g/cc
Loss On Ignition 5.0 %
@Temperature 602 °C
Air; ASTM TGA
 5.0 %
@Temperature 606 °C
Nitrogen; ASTM TGA
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 110 MPaASTM D638
Elongation at Break 0.90 %
Tensile Modulus 18000 MPa
Flexural Strength 158 MPaASTM D790
Flexural Modulus 13000 MPa
Compressive Strength 123 MPaASTM D695
Compressive Modulus 5100 MPa
Coefficient of Friction, Dynamic 0.050
Coefficient of Friction, Static 0.30
 
Thermal PropertiesOriginal ValueComments
CTE, linear 26.0 µm/m-°C
@Temperature 25.0 - 150 °C
ASTM TMA
Specific Heat Capacity 0.280 BTU/lb-°F
@Temperature 70.0 °C
ASTM D648
Thermal Conductivity 5.30 BTU-in/hr-ft²-°F
@Temperature 21.1 °C
ASTM F-433
Deflection Temperature at 1.8 MPa (264 psi) 310 °CASTM D648
 
Descriptive Properties
Wear Rate0.02 in/1000 hrson 1018 steel at 125 psi, 800 ft/min, 350°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PBI Performance Products Celazole® TU-60 Unreinforced Melt Processable Polybenzimidazole
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin
PBI Performance Products Celazole® TF-60 C Carbon Fiber Reinforced Melt Processable Polybenzimidazole
PBI Performance Products Celazole® TF-60 V Glass Fiber Reinforced Melt Processable Polybenzimidazole
Mitsubishi Chemical Advanced Materials Duratron™ CU60 PBI Polybenzimidazole, unfilled, compression molded

PPBIP005 / 140559

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.