  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond 2106T Fast Cure Thixotropic Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 2106T is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. This versatile two-part epoxy system contains no solvents, mixes easily at room temperature, and is suitable for high performance structural bonding applications where the combination of very fast room temperature curing coupled with low shrinkage and excellent mechanical and electrical properties is needed. It develops strong, tough bonds to metals, plastics, glass and glass fabrics, hardboards and forestry products, ceramics, rubber, masonry materials, and other construction materials. When fully cured, TRA-BOND 2106T is an excellent electrical insulator, and provides superior resistance to vapors and gases, water, galvanic action, petroleum fuels, salt solutions, and many other organic and inorganic compounds. TRA-BOND 2106T develops significant properties 1 hour after mixing. However, an extended cure of 4-6 hours at 25°C is required for fully matured bonds. Note: TRA-BOND 2106T develops a high exotherm. Use immediately after mixing. The exothermic reaction begins within 2 minutes after initiating the mixing step, so have everything ready before removing the BIPAX clamp.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccMixed
Solids Content 100 %100 %Reactive Solids Content
Viscosity 3600 cP3600 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 2525After 10 min
 6767After 30 min
 7272After 60 min
Adhesive Bond Strength 1.38 MPa200 psiLap shear, alum to alum
Izod Impact, Notched 1.01 J/cm1.90 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+11 ohm-cm5.00e+11 ohm-cm
Dielectric Constant 4.8
@Frequency 1000 Hz
4.8
@Frequency 1000 Hz
Dielectric Strength 16.1 kV/mm410 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 µm/m-°C
@Temperature 20.0 °C
33.3 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 115 °C239 °F
 150 °C302 °FIntermittent
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 -60.0 °C-76.0 °FIntermittent
Glass Transition Temp, Tg 25.0 °C77.0 °FUltimate Tg
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 65.0 °C
1.00 hour
@Temperature 149 °F
 240 - 360 min
@Temperature 25.0 °C
4.00 - 6.00 hour
@Temperature 77.0 °F
Pot Life 5.0 min5.0 min
 
Descriptive Properties
Color Hazy, Light Straw
Mix Ratio, parts by weight110/93Resin/Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Valley Adhesives EM-500 High Temperature Application Glue Stick
Momentive Performance Materials RTV6445 White Adhesive Sealant, Non-Corrosive High Strength Paste

PTRAC010 / 70938

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.