MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Parkway Products Thixomolded® AM60A Magnesium
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heated to high temperatures and injected into a closed die / mold. Parts from the machine usually need no additional machining, finishing or puttying.

Information provided by Parkway Products.

Key Words: UNS M10600; Mg; ASTM B 94; European EN 1753 MC21230 (Ingot UNS M10601)
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³
Porosity 0.0 - 1.1 %0.0 - 1.1 %
 0.0 - 1.1 %0.0 - 1.1 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 7474
Tensile Strength, Ultimate 221 MPa32000 psi
Tensile Strength, Yield 131 MPa19000 psi
Elongation at Break 4.0 %4.0 %
Modulus of Elasticity 44.8 GPa6500 ksi
Poissons Ratio 0.350.35
Shear Modulus 17.0 GPa2470 ksicalculated
Impact Test 6.10 J4.50 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000100 ohm-cm0.0000100 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 25.6 µm/m-°C
@Temperature 21.1 °C
14.2 µin/in-°F
@Temperature 70.0 °F
Specific Heat Capacity 1.05 J/g-°C0.250 BTU/lb-°F
Thermal Conductivity 62.0 W/m-K430 BTU-in/hr-ft²-°F
Melting Point 616 °C1140 °F
Deflection Temperature at 1.8 MPa (264 psi) >= 371 °C>= 700 °F
Ignition Temperature >= 482 °C>= 900 °Fat One Atmosphere
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 5.5 - 6.5 %5.5 - 6.5 %
Copper, Cu <= 0.35 %<= 0.35 %
Magnesium, Mg 94 %94 %As Remainder
Manganese, Mn 0.13 - 0.60 %0.13 - 0.60 %
Nickel, Ni <= 0.030 %<= 0.030 %
Silicon, Si <= 0.50 %<= 0.50 %
Zinc, Zn <= 0.22 %<= 0.22 %
 
Descriptive Properties
Across Parting Line Dimensions+ 0.0015 inTolerance (0 - 10 in2)
 + 0.0025 inTolerance (11 - 20 in2)
 + 0.004 inTolerance (21 - 50 in2)
 + 0.006 inTolerance (51 - 100 in2)
Flatness Across Largest Dimension+/- 0.001 inTolerance (each inch beyond 1 in)
 +/- 0.002 inTolerance (0 - 3 in)
Linear Dimension in same Die Half+/- 0.0005 inTolerance (0 to 1 in)
 +/- 0.0010 inTolerance (each inch beyond 1 in)
Mil 117B Salt Spray Corrosion4 Mils per Year
Moving Die Component Tolerances+ 0.004 inTolerance (0 - 10 in2)
 + 0.006 inTolerance (11 - 20 in2)
 + 0.008 inTolerance (21 - 50 in2)
 + 0.010 inTolerance (51 - 100 in2)
Shielding Effectiveness 0.020" thk>85 dB100MHz
Shielding Effectiveness 0.050" thk>88 dB100MHz
Surface Finish32 RMS or better
Thickness0.015 - 2.0 in
UL94 Flame Exposure ResultsDNB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Magnesium AM60B-F, Die Cast
Magnesium AM60A-F, Die Cast
ALIMEX ACP 6000 Aluminum Cast Plate
Parkway Products Thixomolded® AZ91D Magnesium
Parkway Products Thixomolded® AM50A Magnesium

MMAM60AT / 12302

Parkway Products

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.