MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Edgetek® PC-15CF-15GF/000 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.37 g/ccASTM D792
Water Absorption 0.15 %@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0010 - 0.0015 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 138 MPaType I, 5.1 mm/min; ASTM D638
Elongation at Break 3.0 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 12400 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 172 MPaASTM D790
Flexural Modulus 12400 MPaASTM D790
Izod Impact, Notched 130 J/m
@Thickness 6.35 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 100 ohm-cm - 1e+05ASTM D257
Surface Resistance 100 ohm - 1e+05ASTM D257
 
Processing PropertiesOriginal ValueComments
Melt Temperature 293 - 327 °C
Mold Temperature 121 °C
Drying Temperature 127 °C
Dry Time 2.00 hour
 
Descriptive Properties
FeaturesFlame Retardant
Filler / ReinforcementGlass\Carbon Fiber Reinforcement
FormsPellets
Generic MaterialPC
Generic NamePolycarbonate (PC)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silberline SilBerCote® PC 1291X
Silberline SilBerCote® PC 4352Z
RTP Company PermaStat® 302 FR Polycarbonate (PC), ESD Protection - Permanently Anti-static - Glass Fiber - Flame Retardant
RTP Company PermaStat® 300 Polycarbonate (PC), ESD Protection - Permanently Anti-static - UL94 HB
RTP Company PermaStat® 1800 A FR Polycarbonate/Acrylic Alloy (PC/PMMA), Flame Retardant - Permanently Anti-static - ESD Protection - UL94 V-0

PH0POL0501 / 145070

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.