MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Michelman® Michem® Emulsion 32535 Nonionic, polyethylene emulsion  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: Nonionic, polyethylene emulsion

Usage: Michem® Emulsion 32535 is best used as an additive in water based coatings where improved slip, rub resistance, hardness and/or block resistance is needed. This wax emulsion can be used as an additive to paper coatings, wood coatings, metal coatings, overprint varnishes, floor polish and other water based coatings where slip and hardness are required, without significant degradation of gloss.

We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foam

Food Contact Information when manufactured in the USA, Belgium and Singapore:
FDA:
175.105: Components of adhesives.

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 - 1.02 g/cc1.00 - 1.02 g/cc
Volatiles 64.5 - 65.5 %64.5 - 65.5 %
pH <= 7.0<= 7.0Recommended pH of system
 9.0 - 10.59.0 - 10.5
Brookfield Viscosity <= 50 cP<= 50 cPSpindle # 2, rpm 60
 
Descriptive Properties
AppearanceLight amber liquid
Emulsifier ChargeNonionic
Solids TypeHigh Density Polyethylene

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Michelman® Michem® Emulsion 93235 Nonionic polyethylene emulsion
Michelman® Michem® Emulsion 52137 Nonionic polyethylene emulsion
Michelman® Michem® Emulsion 47950 Nonionic paraffin emulsion
Michelman® Michem® Emulsion 45745P Nonionic Polyethylene wax emulsion
Michelman® Michem® Emulsion 29730 Nonionic polyethylene emulsion

WMICHEL077 / 134994

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.