MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Silfar® S 184 Silicone Antifoam Agent
Categories: Fluid

Material Notes: Product description: SILFAR® S 184 is a 100% silicone antifoam agent specifically developed for the pharmaceutical and the food processing industries.

Properties: SILFAR® S 184 complies with the requirements set down in the monographs "Simethicone (EP)" and "Simethicone (USP)". SILFAR® S 184 complies with FDA 21 CFR § 173.340 "Defoaming Agents" as "Secondary Direct Food Additive Permitted in Food for Human Consumption". SILFAR® S 184 only contains substances listed in the Directive 95/2/EC and Amendments and is therefore approved as a direct food additive within the EC under observance of the restrictions in force for polydimethylsiloxane (E 900) and silicon dioxide (E 551). SILFAR® S 184 complies with the Recommendations of the BfR concerning the manufacture of essential commodities that have contact with food "XV. Silicones". SILFAR® S 184 and it components meet the criteria for an exemption from the requirements of a tolerance when used as an additive in pesticide formulations to be applied to growing crops or raw agricultural commodities after harvest as specified in 40 CFR 180.950 and 180.960. National regulations applicable in the countries concerned must be observed.

Application: SILFAR® S 184 is used in the pharmaceutical and food industries. SILFAR® S 184, a simethicone is used in antiflatulence and antacid preparations. It works by acting as an antifoam agent to prevent or relieve flatulence in the alimentary canal and by forming a protective lining on e.g. the gastric mucous membrane. It is often combined with fermentation preparations. When administered to patients, preparations containing the antifoam SILFAR® S 184 eliminate any flatulence that might hinder X-ray, ultrasonic or gastroscopic examinations. SILFAR® S 184 may be used to make tablets and coated tablets. SILFAR® S 184 is also an antifoam in fermentation and downstream processes, such as active-ingredient extraction and solvent recovery, especially when USP/EP compliant products are mandatory. SILFAR® S 184 is readily sterilized by heat. In the food industry, SILFAR® S 184 is primarily used when foaming lipophilic systems are present (i.e. for foam control in foodstuffs containing vegatable oils, fats). Furthermore, SILFAR® S 184 is a base material for the production of food-compatible antifoam agents.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³
Volatiles <= 1.0 %<= 1.0 %
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
Active ingredients (%)100
Appearanceviscous, greyish-white, opalescent liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber

PWACK9435 / 204964

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.