MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Santa Maria Wood
Categories: Wood and Natural Products; Wood

Material Notes: Mechanical property data is based on clear, straight-grained specimens from Central or South America.

Key Words: Calophyllum brasiliense, lumber, timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.520 g/cc0.520 g/ccGreen
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 4000 N899 lb (f)Side Hardness, Green
 5100 N1150 lb (f)Side Hardness, 12% Moisture
Modulus of Rupture 0.0724 GPa10.5 ksiStatic Bending, Green
 0.1007 GPa14.61 ksiStatic Bending, 12% Moisture
Flexural Modulus 11.0 GPa1600 ksiStatic Bending, Green
 12.6 GPa1830 ksiStatic Bending, 12% Moisture
Compressive Strength 31.4 MPa4550 psiParallel to Grain, Green
 47.6 MPa6900 psiParallel to Grain, 12% Moisture
Shear Strength 8.70 MPa1260 psiParallel to Grain, Green
 14.3 MPa2070 psiParallel to Grain, 12% Moisture
Work to Maximum Load 0.0720 J/cm³10.4 in-lb/in³Static Bending, Green
 0.108 J/cm³15.7 in-lb/in³Static Bending, 12% Moisture

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTSU143 / 282594

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.