MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT Group QM 264HT 60 Shore A, Addition Cure Moldmaking Material
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QM 264HT is a two-component, room temperature, addition cure, silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin resistance. This material is a good choice for the molding of furniture, picture frames, architectural materials and rubber rollers and belting. QM 264HT is exceptionally good where high durometer and dimensional stability are required.

Key Features:

  • High durometer
  • Casting resin resistance
  • Fast demold time
  • Excellent dimensional stability
Main Applications:
  • Molds for architectural replication
  • Molds for polyester, epoxy resin casting, and rigid or foam polyurethane
  • Molds for technical articles and prototypes
  • Molds for furniture and picture frame replication
  • Rubber rollers and belting

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccQM 264HTB, Uncatalyzed
 1.28 g/ccQM 264HTA, Uncatalyzed
Viscosity 7000 cPQM 264HTB, Uncatalyzed
 110000 cPCatalyzed
 150000 cPQM 264HTA, Uncatalyzed
Linear Mold Shrinkage <= 0.0010 cm/cmCured 3 days at 25°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 53Cured 3 days at 25°C
 63Catalyzed, 30 minutes at 110°C
Tensile Strength 830 psiCured 3 days at 25°C
Elongation at Break 220 %Cured 3 days at 25°C
Tear Strength 116 pliCured 3 days at 25°C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °CCured 3 days at 25°C
Minimum Service Temperature, Air -55.0 °CCured 3 days at 25°C
 
Processing PropertiesOriginal ValueComments
Cure Time 18.0 hourDemold time, Catalyzed
 0.500 hour
@Temperature 110 °C
Catalyzed
 72.0 hour
@Temperature 25.0 °C
Pot Life 160 minCatalyzed
 
Descriptive Properties
ColorBeigeQM 264HTA, Uncatalyzed
 BlackQM 264HTB, Uncatalyzed
 Dark GreyCatalyzed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Elastosil® LR 3003/60 A/B Liquid Silicone Rubber
CHT Group QM 261 60 Shore A, Addition Cure Moldmaking Material
Saint-Gobain COHRlastic® 600 General Purpose Silicone Solid Rubber
Saint-Gobain COHRlastic® 500 General Purpose Silicone Solid Rubber
Overview of materials for Silicone Rubber

PACC2057 / 199445

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.