MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Epoxy Technology EPO-TEK® OE120 Two Component Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Material Description: A two component, opaque epoxy, designed for fiber optics packaging applications. It is a black-colored version of EPO-TEK 353ND-T. It has a high Tg for resisting elevated operating temperatures found in medical fiber optics or hybrid-microelectronic applications.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccPart B
 1.21 g/ccPart A
Particle Size <= 20 µm
Viscosity 12000 - 16000 cP
@Temperature 23.0 °C
20 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
Tensile Modulus 461000 psiStorage
Shear Strength >= 2000 psiLap
 >= 5100 psiDie
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 6.00e+12 ohm-cm
Dielectric Constant 3.47
@Frequency 1000 Hz
Dissipation Factor 0.010
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 28.0 µm/m-°CBelow Tg
 121 µm/m-°CAbove Tg
Maximum Service Temperature, Air 250 °CContinuous
 350 °CIntermittent
Minimum Service Temperature, Air -55.0 °CContinuous
 -55.0 °CIntermittent
Glass Transition Temp, Tg >= 90.0 °CDynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 402 °CDegradation Temperature
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 min
@Temperature 120 °C
minimum
 10.0 min
@Temperature 100 °C
minimum
 20.0 min
@Temperature 80.0 °C
minimum
Pot Life 210 min
Shelf Life 6.00 Month
@Temperature 25.0 °C
 
Descriptive Properties
ColorAmberPart B
 BlackPart A
ConsistencySmooth thixotropic paste
Mix Ratio by Weight10:1
Number of ComponentsTwo
Weight Loss0.07%200°C
 0.38%250°C
 1.12%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® GE120 Electrically and Thermally Insulating Epoxy

PPOXYT140 / 141179

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.