MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Teflon® 807-N PTFE granular molding resin
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Molded

Material Notes: Typical applications are billets for skived tape, basic shapes and moldings by compression and automatic moulding. It can be used for such applications as: seals, valve seats, bearing pads, linings, gaskets, electrical/electronic parts.

Teflon® 807-N is one of DuPont’s free flowing PTFE granular resins designed for compression moulding and ram extrusion (low back pressure).

It offers the excellent combination of properties characteristic of Teflon® fluoropolymer resins: non-ageing characteristics, chemical inertness, exceptional dielectric properties, heat resistance, toughness and flexibility, low coefficient of friction, non-stick characteristics, negligible moisture absorption and excellent weather resistance.

Teflon® 807-N is a multi-purpose PTFE resin which yields high productivity due to its high fill density. It has an excellent combination of handleability, processability, machinability and end-use properties.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.156 g/ccASTM D4894
Apparent Bulk Density 0.950 g/ccASTM D4894
Water Absorption <= 0.010 %ASTM D570
Particle Size 600 µmAverage diameter; ASTM D4894
Linear Mold Shrinkage 0.024 cm/cmDuPont test
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 26.0 MPaASTM D4894
 33.0 MPaSkived Tape, MD (Preforming direction); ASTM D638
 33.0 MPaSkived Tape, CD (Perpendicular to preforming direction); ASTM D638
Elongation at Break 260 %ASTM D4894
 320 %Skived Tape, MD (Preforming direction); ASTM D638
 320 %Skived Tape, CD (Perpendicular to preforming direction); ASTM D638

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Teflon® PTFE 7A Granular Molding Powder
Chemours Teflon® PTFE 8A Granular Molding Powder
Chemours Teflon® PTFE Grade 7B Granular Compression Molding Resin
Chemours Teflon® FEP CX5010 Fluoropolymer Resin
Chemours Teflon® PTFE Grade K-10 Fluoropolymer Resin

PDU9261 / 104598

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.