MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CHT Group QM 262F QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material
Categories: Polymer; Thermoset; Silicone

Material Notes: QM 262F is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin resistance. This material is a good choice for the molding of furniture, picture frames and architectural materials. QM 262F is exceptionally good where high durometer and dimensional stability are required.

Key Features:

  • High Durometer
  • Casting resin resistance
  • Fast demold time
  • Excellent dimensional stability
Main Applications:
  • Molds for architectural replication
  • Molds for polyester, epoxy resin casting, and rigid or foam polyurethane
  • Molds for technical articles and prototype
  • Molds for furniture and picture frame replication

      Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/ccUncatalyzed, QM 262F B
 1.30 g/cc1.30 g/ccBase
Viscosity 2000 cP2000 cPUncatalyzed, QM 262F B
 35000 cP35000 cPcatalyzed with QM 262F B
 55000 cP55000 cPBase
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/incured 72 hrs @ RT
Storage Temperature <= 38.0 °C<= 100 °F12 months
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060cured 72 hrs @ RT
Tensile Strength 6.98 MPa1010 psicured 72 hrs @ RT
Elongation at Break 140 %140 %cured 72 hrs @ RT
Tear Strength 15.8 kN/m90.0 plicured 72 hrs @ RT
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 200 - 300 min3 - 5 hourDemold time, catalyzed with QM 262F B
Pot Life 30.0 min30.0 mincatalyzed with QM 262F B
 
Descriptive Properties
ColorBeigeBase
 Bluecatalyzed with QM 262F B
 Light BlueUncatalyzed, QM 262F B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® 32245 Phenolic, Compression Grade
Rogers Arlon CP-499CA Bulk Compound
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
Overview of materials for Phenolic, Novolac, Mineral/Fiber Filled
Mitsubishi Chemical Advanced Materials TIVAR™ UV UHMW-PE, Natural & Colored Except Black

PACC069 / 22196

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.