MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Extra High Leaded Brass, UNS C35600, H02 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: 1/2 Hard

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Brazing; Fair Suitability – Butt Weld, Capacity for Being Hot Formed; Poor Suitability – Capacity for Being Cold Worked

Common Fabrication Processes: Blanking; Machining; Piercing and Punching; Stamping

Typical uses: Clock and Watch Backs; Clock Gears and Wheels; Clock Plates and Nuts; Channel Plate

Applicable Specifications: Bar – ASTM B121/B121M; Plate - ASTM B121/B121M; Rod, Bar & Shapes – ASTM B453/B453M; Sheet – ASTM B121/B121M; Strip – ASTM B121/B121M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.50 g/cc0.307 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  >= 345 MPa
@Thickness 34.92 mm
>= 50000 psi
@Thickness 1.375 in
 >= 379 MPa
@Thickness 19.0 mm
>= 55000 psi
@Thickness 0.750 in
 >= 393 MPa
@Thickness <=12.7 mm
>= 57000 psi
@Thickness <=0.500 in
Tensile Strength, Yield >= 138 MPa
@Thickness 34.92 mm
>= 20000 psi
@Thickness 1.375 in
for Standard, 0.5% Ext
Elongation at Break  >= 7.0 %
@Thickness <=12.7 mm
>= 7.0 %
@Thickness <=0.500 in
 >= 10 %
@Thickness 19.0 mm
>= 10 %
@Thickness 0.750 in
 >= 15 %
@Thickness 34.92 mm
>= 15 %
@Thickness 1.375 in
Tensile Modulus 96.5 GPa14000 ksi
Modulus of Rigidity 36.5 GPa5300 ksi
Poissons Ratio 0.320.32Calculated
Machinability 100 %100 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000660 ohm-cm0.00000660 ohm-cm26% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.5 µm/m-°C
@Temperature 20.0 - 300 °C
11.4 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 9.65 W/m-K67.0 BTU-in/hr-ft²-°F
Melting Point 888 - 904 °C1630 - 1660 °F
Solidus 888 °C1630 °F
Liquidus 904 °C1660 °F
Annealing Point 427 - 593 °C800 - 1100 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 704 - 788 °C1300 - 1450 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 60 - 63 %60 - 63 %
Iron, Fe <= 0.15 %<= 0.15 %
Lead, Pb 2.0 - 3.0 %2.0 - 3.0 %
Zinc, Zn 34 - 38 %34 - 38 %As Balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC35600x6 / 292940

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.