MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Applied Silicone 40117 High Consistency Rubber, 35 Durometer (HCRA 4735), Implant Grade
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: For Extrusion

Information provided by Applied Silicone Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/cc
Solids Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 30 - 4030 - 40
 3737Typical
Tensile Strength >= 6.21 MPa>= 900 psi
 8.96 MPa1300 psiTypical
Elongation at Break >= 800 %>= 800 %
 1000 %1000 %Typical
200% Modulus 1.03 MPa
@Strain 200 %
150 psi
@Strain 200 %
Tear Strength >= 30.7 kN/m>= 175 pli
 35.1 kN/m200 pliTypical
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min
@Temperature 116 °C
0.167 hour
@Temperature 241 °F
 
Descriptive Properties
Cure SystemPlatinum
Post Cure60 min150°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Elastosil® R plus 4000/40 Silicone Rubber
Overview of materials for Silicone, Molded, Glass Fiber Filled
NuSil MED-4801 Liquid Silicone Rubber - Unrestricted Medical Use
NuSil MED-4735 Two-Part Standard High Consistency Elastomers - Unrestricted Medical Use
Momentive Performance Materials Silplus™ 40 HS High Strength Heat Cured Rubber

PNUSILA914 / 194583

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.