Description: Anionic polyethylene emulsion Usage: Michem® Emulsion 21030 provides abrasion resistance and anti-blocking properties as well as slip resistance when used as an additive in floor polish formulations. We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foam Information provided by Michelman® |