MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ATI Allegheny Ludlum AL 42™ Electrical Alloy, UNS K94100
Categories: Metal; Electronic/Magnetic Alloy; Ferrous Metal

Material Notes: AL 42 alloy is used extensively in the manufacture of sealed beam automobile head lamps, in grommet and pin type glass-metal seals, and in integrated circuit lead frames. It is also the core metal used in the manufacture of Dumet wire. AL 42 alloy has a low expansion coefficient used to match the expansion characteristics of 98% alumina and hard borosilicate glasses. In its various annealed or tempered conditions AL 42 alloy has excellent formability, good stampability, good photoetching characteristics and is solderable. The alloy is fully austenitic at all application temperatures. Where glass-metal sealing is involved, the alloy is usually stabilized with titanium additions to prevent evolution of carbon dioxide bubbles in the glass-metal interface. A titanium stabilized version is available for glass-to-metal seal applications where formation of carbon dioxide bubbles is to be avoided during fabrication.

Information provided by Allegheny Ludlum

Key Words: ASTM F-30 (42)
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.15 g/cc0.294 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 5555Typical Annealed
Tensile Strength, Ultimate 482 MPa69900 psiTypical Annealed
Tensile Strength, Yield 275 MPa
@Strain 0.2 %
39900 psi
@Strain 0.2 %
Typical; Annealed
Elongation at Break 28 %28 %typical in 2"; Annealed
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000660 ohm-cm0.0000660 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  4.00 - 4.70 µm/m-°C
@Temperature 30.0 - 300 °C
2.22 - 2.61 µin/in-°F
@Temperature 86.0 - 572 °F
 6.70 - 7.40 µm/m-°C
@Temperature 30.0 - 500 °C
3.72 - 4.11 µin/in-°F
@Temperature 86.0 - 932 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.0010 %0.0010 %
Carbon, C 0.010 %0.010 %
Chromium, Cr 0.15 %0.15 %
Cobalt, Co 0.0040 %0.0040 %
Iron, Fe 58.4 %58.4 %as balance
Manganese, Mn 0.50 %0.50 %
Nickel, Ni 40.75 %40.75 %
Phosphorus, P 0.010 %0.010 %
Silicon, Si 0.20 %0.20 %
Sulfur, S 0.0070 %0.0070 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schott BOROFLOAT® Borosilicate Float Glass
ATI Allegheny Ludlum AL 36™ Electrical Alloy (Cryogenic and Bimetal) UNS K93600 or UNS K93603
ATI Allegheny Ludlum AL 4750™ Electrical Alloy, UNS K94800 or UNS K95000
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy)
ATI Allegheny Ludlum AL 45™ Magnetic Alloy

NLE42 / 18000

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.