Product Description: EP127 is an injection molding Nylon 66 resin. This resin offers a well-balanced combination of engineering properties characterized by good toughness; high impact; good surface lubricity; abrasion resistance; self-extinguishment. Typical Applications: As an injection molding resin, EP127 is suitable for the production of cable ties and other molding product. Information provided by Zhejiang Haufon New Materials Corp., Ltd. |