MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CHT Group QSil 550LV A/B Addition Cure Potting Material
Categories: Polymer; Thermoset; Silicone

Material Notes: QSil 550LV A and B is a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repairable.

Key Features:

  • 100% solids - no solvents
  • Long pot life
  • Low modulus
  • Good elongation
  • Heat cure required

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/ccUncatalyzed, QSil 550LV A
 1.41 g/cc1.41 g/ccUncatalyzed, QSil 550LV B
Viscosity 1300 cP1300 cPUncatalyzed, QSil 550LV A
 1500 cP1500 cPUncatalyzed, QSil 550LV B
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5858Cure 7 minutes at 150°C
Tensile Strength 2.96 MPa430 psiCure 7 minutes at 150°C
Elongation at Break 85 %85 %Cure 7 minutes at 150°C
Tensile Modulus 0.00352 GPa0.510 ksiYoung's, Cure 7 minutes at 150°C
Tear Strength 3.51 kN/m20.0 pliCure 7 minutes at 150°C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.46e+15 ohm-cm1.46e+15 ohm-cm
Dielectric Constant 3.12
@Frequency 1000 Hz
3.12
@Frequency 1000 Hz
Dielectric Strength 21.2 kV/mm538 kV/in
Dissipation Factor 0.0030
@Frequency 1000 Hz
0.0030
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.370 W/m-K2.57 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Cure Time  10.0 min
@Temperature 150 °C
0.167 hour
@Temperature 302 °F
 15.0 min
@Temperature 125 °C
0.250 hour
@Temperature 257 °F
 30.0 min
@Temperature 100 °C
0.500 hour
@Temperature 212 °F
Gel Time >= 1440 min>= 1440 minCatalyzed
 
Descriptive Properties
ColorBeigeUncatalyzed, QSil 550LV A
 BlackUncatalyzed, QSil 550LV B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Covestro Texin® 945U Urethane Thermoplastic Elastomer
Covestro Texin® 185 Urethane Thermoplastic Elastomer
Covestro Desmopan® 89043D Thermoplastic Polyurethane

PACC2093 / 199481

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.