MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo CALIBRE™ 2060 10 Polycarbonate, Sterilization Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: CALIBRE® 2060 series resins are designed for those applications which use steam or ethylene oxide for sterilization. This material has excellent retention of physical properties and optical clarity when exposed to ethylene oxide. For those applications which use steam sterilization or autoclaving, CALIBRE 2060 series resins offer superior hydrolytic stability for a polycarbonate resin.

Typical applications(1) are hemodialyzers, anesthesia containers, blood oxygenators, arterial filters, intravenous connectors, cardiotomy reservoirs, arteriograph manifolds, blood centrifuge bowls and physiological pressure transducers.

Available Melt Flow Rates: 10, 15.

Associated products:
CALIBRE 2060: without a mold release package
CALIBRE 2061: including a mold release package

(1) NOTICE REGARDING LONG-TERM MEDICAL IMPLANT APPLICATIONS: The Dow Chemical Company does not recommend any medical resin or film product for long-term medical implant applications in humans (more than 72 hours). Further, Dow does nor recommend the use of any medical resin or film product for cardiac prosthetic devices regardless of the time period that the device will be wholly or partially implanted in the body. Such applications include, but are not limited to, pacemaker leads and devices, cardiac prosthetic devices, such as artificial hearts, heart valves, intra-aortic balloon and control systems, and ventricular bypass assist devices. Dow does not recommend any nonmedical grade resin product for use in any human implant applications.

Where available, biocompatibility data relates to resins, not necessarily to fabricated products. Manufacturers of medical devices, equipment and packaging are responsible for determining the suitability of resins for their intended use.

Data provided by Dow Chemical.

This product line was spun off from Dow Chemical to Styron in 2010.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM Data
Water Absorption 0.15 %
Moisture Absorption at Equilibrium 0.32 %Humidity Absorption
Linear Mold Shrinkage 0.0060 cm/cm
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM Data
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118
Tensile Strength, Ultimate 71.0 MPaASTM Data
Tensile Strength, Yield 62.1 MPaASTM Data
Elongation at Break 150 %ASTM Data
Elongation at Yield 6.0 %ISO Data
Tensile Modulus 2.41 GPaASTM Data
Izod Impact, Notched 9.07 J/cmASTM Data
Izod Impact, Unnotched NBASTM Data
Charpy Impact Unnotched NBISO Data
 NBISO Data, Low Temp
Charpy Impact, Notched 1.30 J/cm²ISO Data, Low Temp
 9.00 J/cm²ISO Data
Tensile Impact Strength 526 kJ/m²ASTM Data
Instrumented Impact Total Energy 87.0 J
@Temperature 23.0 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 2.00e+17 ohm-cmASTM Data
Dielectric Constant 2.93
@Frequency 60 Hz
ASTM Data
 2.93
@Frequency 1e+6 Hz
ASTM Data
Dielectric Strength 16.5 kV/mm
Dissipation Factor 0.00050
@Frequency 60 Hz
 0.0017
@Frequency 1e+6 Hz
ASTM Data
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 68.4 µm/m-°C
@Temperature 20.0 °C
ASTM data
Deflection Temperature at 1.8 MPa (264 psi) 128 °CUnannealed; ASTM Data
Vicat Softening Point 156 °C
Flammability, UL94 V-2
@Thickness 3.20 mm
Oxygen Index 26 %
 
Optical PropertiesOriginal ValueComments
Haze 1.1 %
Transmission, Visible 89 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, Optical Grade
Trinseo CALIBRE™ 2061-15 Polycarbonate Resin
Trinseo CALIBRE™ 5051 15 Polycarbonate, 5% Glass Reinforced
Trinseo CALIBRE™ MEGARAD 2081-15 Polycarbonate Resin
Trinseo CALIBRE™ MEGARAD 2081-22 Polycarbonate Resin

PZZDW019 / 34250

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.