MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Glyptal S1300 Silicone Epoxy Coating
Categories: Polymer; Thermoset; Epoxy; Silicone

Material Notes: The Glyptal “S” line (S-1193, S-1194, S-1196, S-1300) are silicone epoxy baking systems that offer a wide array of functional properties on aluminum, magnesium, and steel substrates.

APPLICATION Glyptal “S” Silicone Epoxy coatings include ovens, protective finishes on jet engine components (meets GE Aircraft Specification # F50TF3-S5), aircraft and marine surfaces, solar energy systems, and high-temperature automotive components. The coatings may be applied using conventional spray equipment.

Information provided by Glyptal Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0463 lb/in³
Solids Content 39 %39 %Volume
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 316 °C
@Time 720000 sec
600 °F
@Time 200 hour
No Failure
Flash Point 24.4 °C76.0 °FCC
 
Optical PropertiesMetricEnglishComments
Gloss >= 90 %>= 90 %60°
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 MonthUnopened Can
 
Descriptive Properties
Adhesion1Cross Hatch
Bake Time20-30425°F
Chemical Resistance1Fuel Oil
 6005% Salt Fog
Coverage621 ft²/galDry
Flash Time20
Flexibility.25 inPass
Impact Strength100 lbs - Pass
Pencil Hardness4-5
Viscosity50-60 sec#4 FC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGLYPT937 / 209776

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.