MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Vinnol® H 15/45 M Special Vinyl Chloride Copolymer
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: CAS NO. 32650-26-3

Product description: VINNOL® H 15/45 M SPECIAL is a carboxylatecontaining terpolymer of approx. 84 wt. % vinyl chloride (VC), approx. 15 wt. % vinyl acetate (VAc) and approx. 0.5 wt. % dicarboxylic acid. Its main use is as a binder for surface coating compounds and printing inks.

Properties: VINNOL® H 15/45 M SPECIAL is a thermoplastic, physically drying binder that forms a film when the solvent contained in the formulation has evaporated. Like all VC copolymers, VINNOL® H 15/45 M SPECIAL is extremely tough, showing permanent flexibility, abrasion resistance, little tendency to swell in the presence of water and low gas permeability. It is also highly resistant to oil, grease, dilute aqueous acids, alkalis and saline solutions, as well as to aliphatic hydrocarbons, such as white spirit, and alcohols.

Special features: By virtue of its carboxyl content, VINNOL® H 15/45 M SPECIAL adheres excellently to metal surfaces. It can also be used as a reactant or co-binder in two-pack systems. For example, it may be crosslinked with isocyanates, epoxy or melamine resins. VINNOL® H 15/45 M SPECIAL is characterized by improved thermal stability, making it especially suitable for use in countries with hot climates or as a reactant in applications involving high temperatures, for example in baking finishes.

Application: Typical applications for VINNOL® H 15/45 M SPECIAL:

  • Heat-sealable lacquers
  • Metallic paints
  • Paper and film coatings
  • Printing inks
  • Masonry paints

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.750 g/cc0.0271 lb/in³DIN EN ISO 60
Density 1.37 g/cc0.0495 lb/in³DIN 66137-2
Volatiles <= 1.0 %<= 1.0 %
Particle Size <= 1000 µm<= 1000 µm
Viscosity 50 - 70 cP50 - 70 cP20% solids in MEK; DIN 53015
Molecular Weight 60000 - 80000 g/mol60000 - 80000 g/mol
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 3.0 - 6.03.0 - 6.0[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 74.0 °C165 °FDIN 53765/ISO 11357-5
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 46.8 - 48 %46.8 - 48 %
 
Descriptive Properties
K-Value47-49DIN EN ISO 1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Vinnol® E 15/40 A TF Vinyl Chloride Copolymer
Inovyn Vinidur® 464SZ Polyvinyl Chloride grafted copolymer
Inovyn 460SL Polyvinyl Chloride grafted copolymer
Wacker Vinnol® H 15/45 M Vinyl Chloride Copolymer
Sunoco Ultraclear™ TR3350UC Random Polypropylene Copolymer

PWACK9679 / 205208

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.