Resin Type: Homopolymer Characteristics: Excellent Clarity, Very High Gloss, Medium Slip, No Antiblock, Good Stability at High Drawdown Speeds, Good Printability, Good Heat Seal Characteristics Applications:Bakery Film, Sanitary Film Packaging Processing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.0508 cm. Film properties below based on film thickness of 31.8 µm. Data provided by Chevron Chemical. |