MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DAK Americas Laser+® HS CF746A (D53A) PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Product Description: Laser+® HS CF746A (D53A) polyethylene terephthalate (PET) resin is designed for conversion to PET packaging by injection stretch blow-molding using commercial heat-set technology.

Typical Properties: Laser+® HS CF746A (D53A) is a low DEG moderate CHCD copolymer designed for processes requiring faster crystallization rates, higher glass transition and melting points, but balancing injection molding cycle speed and superior container appearance.

Certification: Laser+® CF746A (D53A) is ideally suited for food packaging applications and is considered in compliance with the Food and Drug Administration (FDA) Food Contact Notification (FCN) 000635, and Health Canada Health Products and Food Branch (HPFB) file KS 07042303 for PET polymers.

Information provided by DAK Americas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 53.0 lb/ft³DAK-QAR-SOP-0018
Particle Size 2500 µmCubical Shape; DAK-QAR-SOP-0017
Particle Mesh Size 24 MeshFines: <0.05%, as packaged; DAK-QAR-SOP-0014
Viscosity Test 80 - 84 cm³/gIntrinsic; DAK-QAR-SOP-0012
Crystallinity >= 35 %DAK-QAR-SOP-0016
 
Thermal PropertiesOriginal ValueComments
Melting Point 244 °Cnominal; DAK-QAR-SOP-0016
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.25 %DAK-QAR-SOP-0013; as packaged
 
Descriptive Properties
Chip Size53-73 chips/gnominal, DAK-QAR-SOP-0015
Color>77.5 CIEL*, DAK-QAR-SOP-0011
 -2.8 -0.2 CIEb*, DAK-QAR-SOP-0011
Compounds<1 ppmAcetaldehyde, DAK-QAR-SOP-0010

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DAK Americas Laser+® W L44A PET
DAK Americas Laser+® HS D59A PET
DAK Americas Laser+® HS Ti818 (G51A) PET
DAK Americas Laser+® W L44B PET
DAK Americas Laser+® W P45A PET

PDAKA019 / 147994

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.