MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Hexcel® Polyspeed® G-EV R68 LT397 Epoxy -Glass Fiber Laminate
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: Polyspeed® G-EV R68 LT397 is a glass fiber epoxy laminate combined with a non woven glass fiber fabric on one side. The laminate is supplied in roll form. Widths are available from 38 - 1270 mm.

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 816 - 1104 MPaValue 0° both sides grounded; EN ISO 527
Tensile Modulus 33.1 - 44.9 GPaValue 0° both sides grounded; EN ISO 527
Tear Strength 0.05304 - 0.07176 kN/mValue 0° both sides grounded; EN ISO 527
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 125 °C
 
Descriptive Properties
Content26-32%Resin
Glass Fiber Reinforcement25 g/m²Glass fiber fabric, Weft
 360 g/m²Glass fiber fabric, Warp
 397 ± 20 g/m²Glass fiber fabric, Areal weight
 680 ± 34 g/m²Glass fiber roving, Areal weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHEXCB9315 / 322471

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.