MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Bada BADAFLEX® UL TPE-S 60A FR01 natural TPE-SEBS
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: UL-listed SEBS compound based on styrene-ethylene / butadiene-styrene copolymer; flame retardant with brominated, ROHS compliant flame retardant.

Information provided by Bada

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060DIN ISO 7619-1
Film Elongation at Break, MD 600 %600 %200 mm/min; DIN 53504
Film Elongation at Break, TD 700 %700 %200 mm/min; DIN 53504
Tear Strength 14.5 kN/m82.7 pliParallel; DIN ISO 34
Compression Set  29 %
@Temperature 23.0 °C,
Time 259000 sec
29 %
@Temperature 73.4 °F,
Time 72.0 hour
DIN ISO 815-1
 42 %
@Temperature 70.0 °C,
Time 86400 sec
42 %
@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815-1
 68 %
@Temperature 100 °C,
Time 86400 sec
68 %
@Temperature 212 °F,
Time 24.0 hour
DIN ISO 815-1
Film Tensile Strength at Break, MD 8.00 MPa1160 psi200 mm/min; DIN 53504
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94  V-0
@Thickness 0.400 mm
V-0
@Thickness 0.0157 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 220 °C374 - 428 °F
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F
Drying Temperature <= 70.0 °C<= 158 °F
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hour
Moisture Content <= 0.10 %<= 0.10 %
 
Descriptive Properties
Overmolding capabilityPP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBADA303 / 287136

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.